41 00... Opening Welded Connections

WARNING: This page is about a different car, the 2013 BMW M3, 2012 BMW M3, and 2011 BMW M3. However, it is still accessible from the selected car via links, so may be relevant.

1. Components made of steel: 

1.1 Opening welding spots (resistance pressure spot welding): 

Sheet steel panels made from high- and super-high-strength materials make great demands on the tools used.

Only with special carbide milling cutters can welding spots be drilled out on these sheet panels.

Use BTR/BOR milling cutters only in conjunction with Vario Drill spot-weld remover. Sourcing reference for spot-weld remover and BTR/BOR milling cutters, see Aftersales Assistance Portal (ASAP) - Service/Technology - Workshop Equipment (Start BMW) - Shop Workshop Equipment or at www.bmwgroup-wep.com.

1.2 Opening MAG weld seams and MIG brazing seams: 

1.3 Opening laser weld seams: 

Laser weld seams are used in the roof outer skin area.

2. Components made of aluminum: 

2.1 Opening MiG weld seams: