When using accelerator (hot processing, 3-hour system)
- Temperature (min. 80 ± 5 °C) of cartridge oven must be checked every morning. Connect temperature sensor to diagnosis system
- Heat adhesive for one hour in cartridge oven (sourcing reference: BMW Parts Department) to 80 ±5 °C
- Write date and time on cartridge when inserting into cartridge oven
- Insufficient heating (< 1 hour) results in the formation of bubbles/blisters (bonding not permitted)
- Temperature < 80 ± 5 °C results in the formation of bubbles/blisters (bonding not permitted)
- Remove hardened adhesive prior to further processing.
- Mistake in mixing in event of an interruption in application > 1 minute (bonding not permitted)
- A sample bead of 50...70 mm must be rejected after an interruption in application
- Expiry dates of accelerator and adhesive must not be more than 3 months apart
- Best before date >3 months results in the formation of bubbles/blisters (gluing/cementing not permitted)
Sealed adhesive:
- May only be stored for a maximum of 8 hours once it has been heated up to 80 ±5 °C
- The adhesive will be damaged if this time is exceeded (bonding not permitted)
- Damaged adhesive must not be used and must be disposed of in compliance with national regulations
- The glue cartridge may only be heated up once
- If the lower label is black, this adhesive may only still be used cold without accelerator while adhering to the expiry date.
IMPORTANT:
Not all window glass may be bonded with accelerator (hot processing).
If hot processing is not permitted, this is described in the relevant document.
If hot processing is not permitted, this is described in the relevant document.